English: A close-up view of the surface of a pipeline showing indications of w:stress corrosion cracking (two clusters of small black lines), as revealed by w:magnetic particle inspection (MPI). The surface was prepared with white contrast paint, and magnetic particles in a liquid suspension were sprayed onto the surface while it was magnetized. Cracks which would normally have been invisible are detectable due to the magnetic particles clustering at the crack openings. The scale at the bottom of the picture is in millimetres. Markings on the pipe were made by a technician for position reference.
Date
Source self-made
Author Davidmack at en.wikipedia
Permission
(Reusing this file)
Licensed under the w:GFDL by the author; Released under the w:GNU Free Documentation License.
Creative Commons CC-Zero This file is made available under the Creative Commons CC0 1.0 Universal Public Domain Dedication.
The person who associated a work with this deed has dedicated the work to the public domain by waiving all of their rights to the work worldwide under copyright law, including all related and neighboring rights, to the extent allowed by law. You can copy, modify, distribute and perform the work, even for commercial purposes, all without asking permission.

Captions

View of the surface of a pipeline showing indications of stress corrosion cracking (two clusters of small black lines)

Items portrayed in this file

depicts

10 July 2012

0.00625 second

6.64 millimetre

image/jpeg

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current16:59, 10 July 2012Thumbnail for version as of 16:59, 10 July 20123,264 × 1,717 (1.53 MB)Davidmack{{Information |Description = A close-up view of the surface of a pipeline showing indications of stress corrosion cracking, as revealed by magnetic particle inspection (MPI). The surface was prepared with white contrast paint, and magnetic par...
The following pages on the English Wikipedia use this file (pages on other projects are not listed):

Global file usage

The following other wikis use this file:

Metadata